Skip to content

Essential cookies keep the website working, analytics is up to you. You can change your choice at any time via Cookie settings in the footer.

Privacy policy

Plate UR™ 65
Plates

Plate UR™ 65

Austenitic 25Cr-21Ni stainless steel with very low carbon for nitric acid service

Key parameters of Plate UR™ 65
Grade 310L NAG / 1.4335 · X1CrNi25-21
Standard EN 10088-2
Dimensions on request
Supplier INDUSTEEL (ArcelorMittal)
Lead time on request

Updated

ISO 9001:2015 EN 10204 3.1 VdTÜV WB 468

Technical data

Technical data

Chemical composition [%]

Chemical composition of Plate UR™ 65 in percent
C ≤ 0.015
Cr ≈ 25
Ni ≈ 21

Mechanical properties

Mechanical properties Plate UR™ 65
Yield strength Rp0.2 ≥ 200 MPa
Tensile strength Rm ≥ 470 MPa
Elongation A5 ≈ 40 %
PREN ≈ 25

High chromium and carbon below 0.015% reduce susceptibility to intergranular corrosion in oxidising media: nitric acid, fertilisers, nuclear fuel reprocessing.

Request a quote: Plate UR™ 65

Fields marked * are required.

Upload drawing / PDF

Drag file here or click to browse

We process the details in your enquiry only to handle it. More information.

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz