Skip to content

Essential cookies keep the website working, analytics is up to you. You can change your choice at any time via Cookie settings in the footer.

Privacy policy

Plate UR™ 28
Plates

Plate UR™ 28

Super-austenitic steel for phosphoric and sulphuric acid

Key parameters of Plate UR™ 28
Grade 28 / 1.4563 · UNS N08028
Standard ASTM A240
Thickness 5–100 mm
Width 1250–3000 mm
Supplier INDUSTEEL (ArcelorMittal)
Lead time 10–14 weeks

Updated

ISO 9001:2015 EN 10204 3.2

Technical data

Technical data

Chemical composition [%]

Chemical composition of Plate UR™ 28 in percent
C ≤ 0.020
Cr 26.0–28.0
Ni 29.5–32.5
Mo 3.0–4.0
Cu 0.6–1.4

Mechanical properties

Mechanical properties Plate UR™ 28
Yield strength Rp0.2 ≥ 220 MPa
Tensile strength Rm 530–730 MPa
Elongation A5 ≥ 35 %
PREN ≈ 34

High nickel and copper content: resistance to hot sulphuric and phosphoric acid.

Request a quote: Plate UR™ 28

Fields marked * are required.

Upload drawing / PDF

Drag file here or click to browse

We process the details in your enquiry only to handle it. More information.

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz