Skip to content

Essential cookies keep the website working, analytics is up to you. You can change your choice at any time via Cookie settings in the footer.

Privacy policy

Plate UR™ 2507W
Plates

Plate UR™ 2507W

Super duplex with tungsten for extreme chloride environments

Key parameters of Plate UR™ 2507W
Grade 2507W / 1.4501 · UNS S32760
Standard EN 10028-7 / ASTM A240
Thickness 5–100 mm
Width 1250–3000 mm
Supplier INDUSTEEL (ArcelorMittal)
Lead time 10–14 weeks

Updated

NORSOK M-630 EN 10204 3.2

Technical data

Technical data

Chemical composition [%]

Chemical composition of Plate UR™ 2507W in percent
C ≤ 0.030
Cr 24.0–26.0
Ni 6.0–8.0
Mo 3.0–4.0
W 0.5–1.0
Cu 0.5–1.0
N 0.20–0.30

Mechanical properties

Mechanical properties Plate UR™ 2507W
Yield strength Rp0.2 ≥ 550 MPa
Tensile strength Rm 750–1000 MPa
Elongation A5 ≥ 25 %
PREN ≥ 40

Tungsten improves pitting corrosion resistance in environments with a high chloride content: offshore fittings.

Request a quote: Plate UR™ 2507W

Fields marked * are required.

Upload drawing / PDF

Drag file here or click to browse

We process the details in your enquiry only to handle it. More information.

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz