Plate SOLEIL™ 4003
Plates

Plate SOLEIL™ 4003

Weldable low-carbon 12.5% Cr stainless steel for load-bearing structures

Key parameters of Plate SOLEIL™ 4003
Grade 4003 / 1.4003 · UNS S41003
Standard EN 10088-2 / ASTM A240
Dimensions on request
Supplier INDUSTEEL (ArcelorMittal)
Lead time on request

Updated

ISO 9001:2015 EN 10204 3.1

Technical data

Technical data

Chemical composition [%]

Chemical composition of Plate SOLEIL™ 4003 in percent
C ≈ 0.020
Cr ≈ 12.5
Ni ≈ 0.5

Mechanical properties (depend on heat treatment)

Mechanical properties (depend on heat treatment) Plate SOLEIL™ 4003
Yield strength Rp0.2 ≥ 280 MPa
Tensile strength Rm ≥ 450 MPa
Elongation A5 ≈ 18 %
PREN ≈ 12

A carbon content of only 0.020% limits hardening of the heat-affected zone of the weld: bridges, architecture, hydrometallurgy, refineries.

Request a quote: Plate SOLEIL™ 4003

Fields marked * are required.

Upload drawing / PDF

Drag file here or click to browse

We process the details in your enquiry only to handle it. More information.

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz