Plates
Plate CryElso™ 201LN
Manganese- and nitrogen-alloyed austenitic stainless steel with a low nickel content
| Grade | 201LN / 1.4371 · UNS S20153 |
|---|---|
| Standard | EN 10088-2 / ASTM A240 |
| Dimensions | on request |
| Supplier | INDUSTEEL (ArcelorMittal) |
| Lead time | on request |
Updated
ISO 9001:2015 EN 10204 3.1
Technical data
Technical data
Chemical composition [%]
| C | ≤ 0.030 |
|---|---|
| Cr | ≈ 16.5 |
| Ni | ≈ 4.7 |
| N | ≈ 0.15 |
| Mn | ≈ 7 |
Mechanical properties
| Yield strength Rp0.2 | ≥ 280 MPa |
|---|---|
| Tensile strength Rm | ≥ 655 MPa |
| Elongation A5 | ≈ 68 % |
| PREN | ≈ 19 |
7% manganese and nitrogen stand in for part of the nickel – 4.7% instead of 8% – at a minimum tensile strength of 655 MPa: cryogenic tanks and refineries.
Request a quote: Plate CryElso™ 201LN
Sales department
Usually within 24 hours, depending on the complexity of the specification
+420 224 234 322 pragointer@pragointer.cz