Skip to content

Essential cookies keep the website working, analytics is up to you. You can change your choice at any time via Cookie settings in the footer.

Privacy policy

Bar 61SiCr7 +Ti
Bars

Bar 61SiCr7 +Ti

Silicon-chromium spring steel with titanium for highly stressed springs

Key parameters of Bar 61SiCr7 +Ti
Grade 61SiCr7 +Ti
Standard EN 10089 (modified)
Diameter Ø 20–100 mm
Length 3000–12000 mm
Supplier Asil Çelik
Lead time 8–12 weeks

Updated

EN 10204 3.1

Technical data

Technical data

Chemical composition [%]

Chemical composition of Bar 61SiCr7 +Ti in percent
C 0.56–0.64
Si 1.20–1.60
Cr 0.60–0.90
Ti microalloyed

Mechanical properties

Mechanical properties Bar 61SiCr7 +Ti
Yield strength Rp0.2 ≥ 1300 MPa (quenched and tempered)
Tensile strength Rm 1500–1700 MPa

Titanium refines the grain and increases fatigue strength: valve and suspension springs for the automotive industry.

Request a quote: Bar 61SiCr7 +Ti

Fields marked * are required.

Upload drawing / PDF

Drag file here or click to browse

We process the details in your enquiry only to handle it. More information.

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz