Skip to content

Essential cookies keep the website working, analytics is up to you. You can change your choice at any time via Cookie settings in the footer.

Privacy policy

Bar 39MnCrB6
Bars

Bar 39MnCrB6

Boron case-hardening / quench-and-temper steel with high hardenability

Key parameters of Bar 39MnCrB6
Grade 39MnCrB6
Standard EN 10083-3 (equivalent)
Diameter Ø 101–220 mm
Length 3000–12000 mm
Supplier Asil Çelik
Lead time 8–12 weeks

Updated

EN 10204 3.1

Technical data

Technical data

Chemical composition [%]

Chemical composition of Bar 39MnCrB6 in percent
C 0.35–0.42
Mn 1.10–1.40
Cr 0.35–0.55
B 0.0008–0.005

Mechanical properties

Mechanical properties Bar 39MnCrB6
Yield strength Rp0.2 ≥ 650 MPa
Tensile strength Rm 900–1050 MPa

The boron addition significantly increases hardenability at a low alloying cost: high-strength fasteners.

Request a quote: Bar 39MnCrB6

Fields marked * are required.

Upload drawing / PDF

Drag file here or click to browse

We process the details in your enquiry only to handle it. More information.

Sales department

Usually within 24 hours, depending on the complexity of the specification

+420 224 234 322 pragointer@pragointer.cz